What is Multilayer Engineered Flooring?
1.Structure:
1.1.The Engineered Flooring first layer is usually with UV coating of natural oil.
1.2.The second layer is the hardwood top layer and it is also called veneer layer and it can be oak, walnut, maple, birch, etc. And the veneer thickness is usually 2mm, 3mm, 4mm, etc.
1.3.The third layer is the plywood core layer and this layer uses different species of veneers forming plywood, such eucalyptus, poplar, birch.
1.4.The fourth layer is the backing layer and it is to provide stability to the board and its species is usually poplar.
2.Specifications
Flooring Type | Prefinished | Species | Maple/Hard Maple |
Color | Brown | Shade | Medium/Neutral Shade |
Finish Type | Urethane | Gloss Level | Low-Gloss |
Application | Residential | Core Type | Multi-Ply |
Profile | Tongue & Groove | Edge Type | French Bleed |
Maximum Length (in.) | 48 | Minimum Length (in.) | 20 |
Average length (in.) | 33 | Width (in.) | 5 |
Thickness (in.) | 0.55 | Radiant Heat Compatible | No |
Below Grade | Yes | Installation | Floating, Glue Down, Nail Down, Staple Down |
Certification | CARB II | Wear Layer Thickness (mm) | 3 |
Surface Finish | Distressed, Handscraped | Finish Warranty (in years) | 25 years |
Structural Warranty (in years) | 25 Years | Country of Origin | China |
Packaging Dimensions (inches) | Height: 4.75 Length: 84 Width: 5 | Product Dimensions | Height: 9/16″ Length: 15 3/4 – 47 1/4″ Width: 5″ |
Sqft / Box | 17.5 | Proposition 65 | Attention California Residents |
3 Layer Engineered Structure
Multilayer Engineered Structure
Engineered Flooring Advantage
Specifications
Wood Flooring species: | Oak, Maple, Birch, Cherry ,Teak, Ash, Rosewood, Walnut, etc. | |
Origin: | Europe, America, China | |
Dimensions: | Length: From 300mm to 2200mm | |
Width: From 60mm to 600mm | ||
Thickness: From 7mm to 22mm | ||
Structure: | Multilayer or 3 Layers | |
Top layer: | 0.2mm/0.6mm/2mm/3mm/4mm/5mm/6mm | |
Veneer Grade: | AB/ABC/ABCD | |
Moisture content | 8% +/-2 | |
Joint system | T&G | |
Core material: | Eucalyptus , Poplar ,Birch | |
Glue: | Dynea Phenolic aldehyde resin (CARB P2, E0) | |
Color: | Medium, Light, Natural, Dark | |
Surface treatments: | Smooth/wire-brushed/hand-scraped/distressed/carbonized/smoked | |
Finish: | Treffert UV coating, OSMO natural oil | |
Installation: | Glue, float or nail down | |
Package: | Cartons or Pallet | |
Certificate: | CE,SGS,FSC,PEFC, ISO9001,ISO140001 | |
OEM: | Offered |
What is engineered wood flooring advantage than hardwood flooring ?
Multi-layer solid wood flooring is a new type of flooring between solid wood flooring and laminate flooring, and is a new trend in floor purchase. Multi-layer solid wood flooring retains all the advantages of natural solid wood flooring. It not only has the natural texture and elasticity of solid wood flooring, but also overcomes the common problems of natural solid wood flooring that is easy to swell and shrink. It has the characteristics of anti-deformation, corrosion resistance and easy cleaning.
Secondly, choose whether the size of the product is consistent with the length, width, and thickness of the size you purchased, and then check whether the dimensional tolerance of the product is consistent with the purchased grade. The measurement method can take multiple pieces of floor in the same packing box and assemble it by yourself. After assembling, observe whether the tenon and groove are tightly combined. At the same time, you can touch the floor after splicing to see if it is irregular. If there is a prominent hand feeling phenomenon , Indicating that the product is unqualified. After touching it by hand, pick up two assembled multi-layer solid wood floors and shake them in your hands to see if they are loose.
Finally, select the intrinsic quality, which is a key indicator of multilayer solid wood flooring. It can be seen from the water absorption thickness expansion rate that its waterproof and moisture-proof performance, the lower the better, the best is less than 2%, followed by less than 5%. Pyrotechnics are burned on the surface. If there are no traces, the fireproof coefficient is higher. The formaldehyde content is an index that cannot be ignored. According to national regulations, the formaldehyde content per 100g floor shall not exceed 9mg. “Three-point floor and seven-point installation”, so it is recommended to choose DEGE brand flooring when choosing multilayer solid wood flooring
Design Type
Click Type
Finish Type
Veneer Grade
How to Distinguish Engineered Flooring Veneer Grade
1. Distinguish Method
Grade A: knots are not allowed;
Grade B:Quantity of knots per pc: 1-3pcs and the diameter of knots whose color are black is within 8mm and diameter of knots whose color are nearly same as veneer is within 10mm;
Grade C: Quantity of knots per pc: 1-3pcs and the diameter of knots whose color are black is within 20mm and diameter of knots whose color are nearly same as veneer is within 25mm; In addition, 20% of white edge of plank width is allowed and medium color variation is allowed;
Grade D: Quantity of knots per pc: 1-3pcs and the diameter of knots whose color are black is within 30mm and diameter of knots whose color are nearly same as veneer is unlimited; In addition, length of crack is within 30cm and severe color variation is allowed;
2.Percentage
ABC Grade: Percentage of grade AB: 15%, Percentage of grade C: 85%;
ABCD Grade: Percentage of grade AB: 20%, Percentage of grade C: 50%, Percentage of grade D: 30%
3.Picture
Certificate
Product Process
Our Market
Applications
Project 1
Project 2
Product detail pictures:
Related Product Guide:
With sophisticated technologies and facilities, strict top quality handle, reasonable value, exceptional support and close co-operation with clients, we are devoted to furnishing the ideal worth for our clients for Factory Cheap Hot Bamboo Parquet Floor - 12mm Wirebrushed Ash Wood Flooring – DEDGE , The product will supply to all over the world, such as: Bolivia, Irish, Venezuela, Our products are produced with the best raw materials. Every moment, we constantly improve the production programme. In order to ensure better quality and service, we have been focusing on the production process. We have got high praise by partner. We are looking forward to establishing business relationship with you.
By Helen from Bhutan - 2017.06.16 18:23
We feel easy to cooperate with this company, the supplier is very responsible, thanks.There will be more in-depth cooperation.
By Ellen from Norwegian - 2018.04.25 16:46